Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00320 ohm-cm | 0.00320 ohm-cm | |
Poco Graphite ZEE-2 Ion Implant Grade Graphite ZEE is a hard, wear-resistant material. This next generation ion implant material offers improved performance through the entire range of low to high-energy implants. POCO ZEE is high-purity, isotro.. |