Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 51045 PET, Pellet, Injection Molded, Black  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 51045 PET, Pellet, Injection Molded, Black  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 51045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is It is UL listed and available in black only.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.72 g/cc
0.0621 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 186.3 MPa
27020 psi
ASTM D638
Elongation at Break 1.63 %
1.63 %
ASTM D638
Tensile Modulus 16.71 GPa
2424 ksi
ASTM D638
Flexural Yield Strength 266 MPa
38600 psi
ASTM D790
Flexural Modulus 14.43 GPa
2093 ksi
ASTM D790
Compressive Yield Strength 192.9 MPa
27980 psi
ASTM D695
Izod Impact, Notched 0.810 J/cm
1.52 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.920 J/cm²
4.38 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 229 °C
444 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 6.97e+16 ohm-cm
6.97e+16 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 16.8 kV/mm
427 kV/in
Short Time; ASTM D149
Dissipation Factor 0.012

@Frequency 1e+6 Hz
0.012

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 80 sec
80 sec
ASTM D495
Comparative Tracking Index 250 V
250 V
ASTM D3638
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved