Tensile Strength, Ultimate 186.3 MPa
27020 psi
ASTM D638
Plenco 51045 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is It is UL listed and available in black only.Information supplied b..