Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.920 J/cm² | 4.38 ft-lb/in² | ASTM D256 |
Plenco 51045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is It is UL listed and available in black only.Information supplied b.. |
|||
Charpy Impact, Notched | 0.920 J/cm² @Temperature 23.0 °C |
4.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFG20-FN00N1 Nylon 6 20% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 0.920 J/cm² | 4.38 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Charpy Impact, Notched | 0.920 J/cm² | 4.38 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Charpy Impact, Notched | 0.920 J/cm² | 4.38 ft-lb/in² | ISO 179 |
BASF Ultramid® B3WG7 BK00564 35% Glass Filled PA6 (Dry) Ultramid B3WG7 BK00564 is a 35% glass fiber reinforced, pigmented black, injection molding PA6 grade for highly rigid, dimensionally stable components which are resistant to high
temperature aging a.. |
|||
Charpy Impact, Notched | 0.920 J/cm² | 4.38 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |