Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | ASTM D648 |
Polymer Resources NY66-IMG13-[color]H Nylon, 13% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | Unannealed; ISO 75-2/C |
Pasargad Polymer Peyvand Pasamid 3P-H1145B Nylon 6, 45% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 - 260 °C | 444 - 500 °F | Average value: 246 °C Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP RX05495 PA 66 LNP LUBRICOMP* RX05495 is a compound based on Nylon 66 resin containing Glass Bead, Graphite, Glass Fiber. Added features of this material include: Easy Molding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M36 HS BK 36% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 36% Filler by Weight and Mineral Filler, 36% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 B1 BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearan.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 HS L NAT 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 L BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PET GF55 X 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66 LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C @Thickness 3.20 mm |
444 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66 LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C @Thickness 3.20 mm |
444 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX RNX130 PPE+PS+PA 30% glass reinforced PPE+PS+PA alloy for automotive and nonautomotive applications. Recycle grade in black/gray only. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6/6 GF30 FR HS2 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp RFB53U PA 66 (Europe-Africa-Middle East) LNP*THERMOCOMP*RFB53U is a compound based on PA 66 resin containing Glass Bead, Glass Fiber. Added features include: UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle E.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Asia Pacific) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | ASTM D648 |
PlastxWorld Veroplas PB3400 Nylon 66 general purpose, 40% glass filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | ASTM D648 |
PlastxWorld Veroplas PB3500 Nylon 66 general purpose, 50% glass filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | ASTM D648 |
E-Polymers TEKASTER® F615G55 55% Glass Fiber Reinforced High Modulus PET Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | ASTM D648 |
Ashley Polymers Ashlene® 525LD-13G Nylon 66, 13% Glass Reinforced High impact Nylon 66 reinforced with 13% glass fibers.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | ASTM D648 |
A. Schulman ComAlloy E-16674B PPS, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | ASTM D648 |
Solvay Specialty Polymers Xydar® M-345 Liquid Crystal Polymer, 45% Mineral Filled
(discontinued **) XYDAR M-345 Liquid Crystal Polymer (LCP) is a 45% mineral-filled injection molding grade with exceptional moldability. XYDAR M-345 resin can fill very thin walls over long flow lengths with little o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 756 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 444 °F | ASTM D648 |
Plenco 50045 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |