Plenco 50335 PET, Pellet, Injection Molded, Natural Color  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 50335 PET, Pellet, Injection Molded, Natural Color  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.63 g/cc
0.0589 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.0024 cm/cm
0.0024 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 123.9 MPa
17970 psi
ASTM D638
Elongation at Break 1.99 %
1.99 %
ASTM D638
Flexural Yield Strength 187.2 MPa
27150 psi
ASTM D790
Flexural Modulus 8.74 GPa
1270 ksi
ASTM D790
Compressive Yield Strength 170.7 MPa
24760 psi
ASTM D695
Izod Impact, Notched 0.540 J/cm
1.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 9.14e+15 ohm-cm
9.14e+15 ohm-cm
ASTM D257
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 19.4 kV/mm
493 kV/in
Short Time; ASTM D149
Dissipation Factor 0.015

@Frequency 1e+6 Hz
0.015

@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 200 V
200 V
ASTM D3638