Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0024 - 0.0030 cm/cm @Thickness 3.17 mm |
0.0024 - 0.0030 in/in @Thickness 0.125 in |
|
Ovation Polymers OPTRENE 20GF Polypropylene, 20% Glass Reinforced Properties of chemically coupled glass reinforced (20%) polypropylene with high strength and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All .. |
|||
Linear Mold Shrinkage | 0.0024 - 0.0030 cm/cm @Thickness 3.17 mm |
0.0024 - 0.0030 in/in @Thickness 0.125 in |
|
Ovation Polymers OPTRENE 30GF Polypropylene, 30% Glass Reinforced Properties of chemically coupled glass reinforced (30%) polypropylene with high strength and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All .. |
|||
Linear Mold Shrinkage | 0.0024 cm/cm | 0.0024 in/in | ASTM D955-89 |
Multibase Multi-ABS 8933 Black Ash is 28% per ASTM D-5630-94.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.0024 cm/cm | 0.0024 in/in | Bayer Test |
Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, 15% Milled Glass Filled, MDI-based 2-Component Liquid System 0.25 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – C.. |
|||
Linear Mold Shrinkage | 0.0024 - 0.0036 cm/cm | 0.0024 - 0.0036 in/in | IS 13411-1992 |
Amity Thermosets ATS 132 Phenolic Molding Organic, inorganic, and graphite Filler, Compression Molded Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti.. |
|||
Linear Mold Shrinkage | 0.0024 cm/cm | 0.0024 in/in | ATM D955 |
Plenco 50335 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |