Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 50030 PET, Pellet, Injection Molded, Black  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 50030 PET, Pellet, Injection Molded, Black  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0013 cm/cm
0.0013 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 147.8 MPa
21440 psi
ASTM D638
Elongation at Break 1.77 %
1.77 %
ASTM D638
Tensile Modulus 10.56 GPa
1532 ksi
ASTM D638
Flexural Yield Strength 215.6 MPa
31270 psi
ASTM D790
Flexural Modulus 10.27 GPa
1490 ksi
ASTM D790
Compressive Yield Strength 174.6 MPa
25320 psi
ASTM D695
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 9.23e+17 ohm-cm
9.23e+17 ohm-cm
ASTM D257
Dielectric Constant 3.3

@Frequency 1e+6 Hz
3.3

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 16.3 kV/mm
414 kV/in
Short Time; ASTM D149
17.0 kV/mm
432 kV/in
Step by Step; ASTM D149
Dissipation Factor 0.012

@Frequency 1e+6 Hz
0.012

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 60 sec
60 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638