Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastics Group Polifil® RMC-40V 40% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® RMC-40V 40% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polifil® RMC-V series compounds are high impact, UV stabilized polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, these compounds retard dust and maintain their original state and color for many years.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Filler Content 40 %
40 %
ASTM D2584
Linear Mold Shrinkage 0.010 cm/cm

@Thickness 1.59 mm
0.010 in/in

@Thickness 0.0625 in
ASTM D955
Melt Flow 16 - 20 g/10 min
16 - 20 g/10 min
230/2.16; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength at Break 21.7 MPa
3150 psi
ASTM D638
Flexural Modulus 2.48 GPa
360 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
At 73°F; ASTM D256
Izod Impact, Unnotched NB
NB
At 73°F; ASTM D256
Gardner Impact 5.42 J
4.00 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ASTM D648