Material Notes:
COPYLENE™ CH014 is a polypropylene homopolymer resin designed for extrusion applications. Applications: Raffia/Tapes/Strapping; Geotextile & Agriculture; Nets. Equivalent to Pro-fax® HL781GInformation provided by Phillips 66.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.1 MPa
4800 psi
2 in/min; ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Descriptive Properties Value Comments
Process Extrusion
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution