Permabond Anti-Seize Compound Lubricant

Category Fluid , Lubricant
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond Anti-Seize Compound Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Permabond Anti-Seize is a superior grade assembly compound and high pressure lubricant. This high quality aluminum, copper and graphite based antiseize formula has unique particle shapes suspended in special carriers. It will protect metal parts under extreme heat, pressure and contaminating conditions to 2000°F (1095°C). AntiSeize is designed with ultra-fine metallic and graphite particles enhancing a longer lasting protective film, resisting washout, burn-off and corrosion. Features & Benefits: Protects against rust and corrosion Reduces friction – provides constant torque/tension Speeds assembly / disassembly Prevents seizing, galling and cold welding Retards galvanic action between dissimilar metals Resists salt water corrosion Compatible with all types of metals and most plastics Non-hardening and non-dripping Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Solids Content 42 %
42 %
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Coefficient of Friction 0.10
0.10
Penetration 320 - 350
320 - 350
100-3000 strokes; ASTM D217-60T
Oil Separation <= 1.0 %

@Temperature 70.0 °C,
Time 108000 sec
<= 1.0 %

@Temperature 158 °F,
Time 30.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1095 °C
2003 °F
Minimum Service Temperature, Air 184 °C
363 °F
Flash Point 177 °C
351 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Silver Grey, Homogenous Paste