Thermal Properties Metric English Comments
Minimum Service Temperature, Air 184 °C
363 °F
Permabond Anti-Seize Compound Lubricant
Permabond Anti-Seize is a superior grade assembly compound and high pressure lubricant. This high quality aluminum, copper and graphite based antiseize formula has unique particle shapes suspended i..