Description: MoldStar® 18 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: SlidesGibsWear PlatesMold Locking DevicesSleeve BearingsGuide Pin BushingsGuide RailsInformation provided by Performance Alloys.
Physical Properties Metric English Comments
Density 7.45 g/cc
0.269 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 192
192
3000kg
Hardness, Rockwell B 92
92
Tensile Strength at Break 724 MPa
105000 psi
Tensile Strength, Yield 359 MPa
52000 psi
Elongation at Break 14 %
14 %
in 2"
Compressive Strength 262 MPa
38000 psi
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 °C
9.00 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 62.3 W/m-K

@Temperature 15.6 °C
432 BTU-in/hr-ft²-°F

@Temperature 60.0 °F
Component Elements Properties Metric English Comments
Aluminum, Al 10.5 %
10.5 %
Copper, Cu 85.5 %
85.5 %
Iron, Fe 3.5 %
3.5 %
Other 0.50 %
0.50 %
Descriptive Properties Value Comments
Thermal diffusivity at 68°F 0.97 ft²/hr