Thermal Properties Metric English Comments
Thermal Conductivity 62.3 W/m-K

@Temperature 15.6 °C
432 BTU-in/hr-ft²-°F

@Temperature 60.0 °F
Performance Alloys MoldStar® 18 (PAS 18) Bronze Mold Alloy
Description: MoldStar® 18 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: SlidesGibsWear PlatesMold Locking DevicesSl..
Thermal Conductivity 62.3 W/m-K
432 BTU-in/hr-ft²-°F
Eagle Brass 521 Phosphor Bronzes 8% C, 1/2 Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Thermal Conductivity 62.3 W/m-K
432 BTU-in/hr-ft²-°F
Eagle Brass 521 Phosphor Bronzes 8% C, 1/4 Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Thermal Conductivity 62.3 W/m-K
432 BTU-in/hr-ft²-°F
Eagle Brass 521 Phosphor Bronzes 8% C, 3/4 Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Thermal Conductivity 62.3 W/m-K
432 BTU-in/hr-ft²-°F
Eagle Brass 521 Phosphor Bronzes 8% C, Annealed
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Thermal Conductivity 62.3 W/m-K
432 BTU-in/hr-ft²-°F
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Thermal Conductivity 62.3 W/m-K
432 BTU-in/hr-ft²-°F
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Spring
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Thermal Conductivity 62.3 W/m-K
432 BTU-in/hr-ft²-°F
Eagle Brass 521 Phosphor Bronzes 8% C, Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Thermal Conductivity 62.3 W/m-K
432 BTU-in/hr-ft²-°F
Eagle Brass 521 Phosphor Bronzes 8% C, Spring
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..