Material Notes:
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 3.65 - 4.15 g/cc
3.65 - 4.15 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 68 - 82
68 - 82
Tensile Strength at Break >= 1.38 MPa
>= 200 psi
ASTM D412
Elongation at Break >= 200 %
>= 200 %
ASTM D412
Tear Strength 13.125 kN/m
74.891 pli
Compression Set 40 %
40 %
70 hrs @ 100°C; ASTM D395 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.0060 ohm-cm
0.0060 ohm-cm
as supplied without pressure sensitive adhesive
Shielding Effectiveness >= 85 dB
>= 85 dB
2 GHz (Plane Wave); MIL-G-83528
>= 85 dB
>= 85 dB
10 GHz (Plane Wave); MIL-G-83528
>= 100 dB
>= 100 dB
500 MHz (E Field); MIL-G-83528
>= 105 dB
>= 105 dB
100 MHz (E Field); MIL-G-83528
Descriptive Properties Value Comments
Binder EPDM
Filler Ag/Ni
Heat Aging ohm-cm max 0.0125