Plenco 2300 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2300 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654. 02300 is available in black, brown, red, or green.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Water Absorption 0.38 %
0.38 %
ASTM D570
Linear Mold Shrinkage 0.0047 cm/cm
0.0047 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 93
93
ASTM D785
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 0.79 %
0.79 %
ASTM D638
Tensile Modulus 9.00 GPa
1310 ksi
ASTM D638
Flexural Strength 97.0 MPa
14100 psi
ASTM D790
Flexural Modulus 8.40 GPa
1220 ksi
ASTM D790
Compressive Strength 227 MPa
32900 psi
ASTM D695
Izod Impact, Notched 0.173 J/cm
0.324 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.190 J/cm²
0.904 ft-lb/in²
ASTM D256
Impact 115
115
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 76.0 µm/m-°C

@Temperature 40.0 - 130 °C
42.2 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.360 W/m-K

@Temperature 100 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 202 °C
396 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 168 °C
334 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 25.5 %
25.5 %
ASTM D2863
Shrinkage 0.173 %
0.173 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.20e+12 ohm-cm
2.20e+12 ohm-cm
ASTM D247
Dielectric Constant 4.8
4.8
ASTM D150
Dielectric Strength 15.5 kV/mm
394 kV/in
Short Time; ASTM D149
Dissipation Factor 0.039
0.039
ASTM D150
Arc Resistance 98 sec
98 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638