Parker Chomerics C-Wings Heat Spreaders

Category Other Engineering Material
Manufacturer Parker Chomerics
Trade Name C-Wings
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics C-Wings Heat Spreaders.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreaders consist of 5oz. [0.007inch/0.18mm thick] flexible copper foil between electrically insulating films. High strength silicone PSA (pressure-sensitive adhesive) provides a strong bond to the component. The compliant nature of these “thermal wing” heat spreaders permits nearly 100% adhesive contact with non-flat package surfaces, optimizing thermal and mechanical performance.Features/Benefits: Component junction temperature reduction of 10-20°C is common, Easily added to existing designs to lower component temperatures and improve reliability, Custom shapes available for complex designs, Used where localized sensitivity to EMI (electromagnetic interference) exists, Low profile, and Peel and stick application.Typical Applications: Microprocessors, Memory modules, Laptop PC’s and other high density, hand held portable electronics, and High speed disk drives.Information provided by Chomerics
Physical Properties Metric English Comments
Thickness 76.0 microns
2.99 mil
PSA Thickness; Visual
1530 microns
60.2 mil
Total; ASTM D376
1600 microns
63.0 mil
Thermal Conductor
Mechanical Properties Metric English Comments
Shear Strength 0.0230 MPa

@Temperature 100 °C,
Time 3600 sec
3.34 psi

@Temperature 212 °F,
Time 1.00 hour
Lap; ASTM D1000
0.414 MPa

@Temperature 25.0 °C,
Time 3600 sec
60.0 psi

@Temperature 77.0 °F,
Time 1.00 hour
Lap; ASTM D1000
Peel Strength 0.216 kN/m
1.23 pli
60 min, 100°C, ASTM B571/D2861
0.432 kN/m
2.46 pli
1 min, 25°C, ASTM B571/D2861
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 1.00e+14 ohm-cm
<= 1.00e+14 ohm-cm
ASTM D149
Dielectric Constant 9.1

@Frequency 1.00e+9 Hz
9.1

@Frequency 1.00e+9 Hz
ASTM D150
Dielectric Strength 12.0 kV/mm
305 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 1.00e+6 Hz
0.0010

@Frequency 1.00e+6 Hz
Chomerics Test
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Chomerics
Descriptive Properties Value Comments
Color Tan
Creep Adhesion 135°C, 3kPa, on aluminum, P.S.T.C. No. 7
Pressure-Sensitive Adhesive Type Silicone based
Thermal Conductor Aluminum Oxide
Weight, oz/inch2 0.76