Mechanical Properties Metric English Comments
Peel Strength 0.216 kN/m
1.23 pli
60 min, 100°C, ASTM B571/D2861
Parker Chomerics C-Wings Heat Spreaders
Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreade..
Peel Strength 0.216 kN/m
1.23 pli
60 min, 100°C, ASTM B571/D2861
Parker Chomerics T-Wings Heat Spreaders
Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreade..