Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1530 microns | 60.2 mil | Total; ASTM D376 |
Parker Chomerics C-Wings Heat Spreaders Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreade.. |