Material Notes:
Non-Hal FR-PC with High HDT, high impact and improved processability. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.0 MPa
6670 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 52.0 MPa
7540 psi
50 mm/min; ASTM D638
Elongation at Break 34 %
34 %
50 mm/min; ASTM D638
Tensile Modulus 1.58 GPa
229 ksi
50 mm/min; ASTM D638
Flexural Strength 77.0 MPa
11200 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.95 GPa
283 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 6.50 J/cm
12.2 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 124 °C

@Thickness 3.20 mm
255 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0
V-0