Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
Nylene® Norpex® AX235 PPE (Polyphenylene Ether) Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® INP564 ABS+SAN SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS Automotive applications: High impact and ductility to -22F for interior trim and instrument panel applications. |
|||
Tensile Strength, Yield | 52.0 MPa @Thickness 6.35 mm |
7540 psi @Thickness 0.250 in |
ASTM D638 |
SABIC Innovative Plastics Lexan® FL910 PC Various weight reductions at 0.250"" (6.35 mm) wall, 10% GR. High flexural strength and modulus, impact/heat resistant. V-0/5V at 0.250"" (6.35 mm). |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® ML7647K PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
Ineos Nova 1280 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 150°C for 1,000 hrs; ASTM D1458 |
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Tensile Strength, Yield | 52.0 MPa @Thickness 3.20 mm |
7540 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUMID HI1202B(W) PA66, High Impact Feature: Injection Molding, PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Tensile Strength, Yield | 52.0 MPa @Thickness 3.20 mm |
7540 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® GP1000W PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
Ineos Nova 1290 High Heat Crystal Polystyrene Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527-1/-2 |
Mitsubishi Xantar® MX 1021 FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Strength, Yield | 52.0 MPa @Thickness 3.20 mm |
7540 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HR2100D PP+GF17% Description: Injection Molding, PP+GF17%, General PurposeApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 165997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DX94375H PC LNP* LUBRICOMP* DX94375H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V9500GW PET+PC (Europe-Africa-Middle East) Unfilled Flameretardant PET/PC blend for GWIT.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON TE002 PU LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 67002XXH PBT+PC LNP* THERMOCOMP* 67002XXH is a compound based on PBT+PC containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features inc.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HP-1011 PC/ABS, Unreinforced Material with superior flowability and small gas generation that can be used in the exterior material of mobile phonesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
Teknor Apex Sinpolene GPP1610 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 10% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. .. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | 50 mm/min |
Arkema Group Orgalloy® RS 6600 Nylon 66 Alloy, Rigid Grade (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | GB/1040 |
Zhejiang Juner PC-3-1 Alloy Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, Conditioned Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Tensile Strength, Yield | 52.0 MPa | 7540 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |