Polymer Property : Flexural Modulus = 1.95 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.95 GPa
283 ksi
Plastcom SLOVALEN PQ 81 T 30 PP, 30% mineral filling
FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene..
Flexural Modulus 1.95 GPa
283 ksi
1.3 mm/min, 50 mm span; ASTM D790
Ovation Polymers Nima™ NH PC151 Polycarbonate
Non-Hal FR-PC with High HDT, high impact and improved processability. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared accordi..
Flexural Modulus 1.95 GPa
283 ksi
0.1 in/min; 0.250" thickness; ASTM D-790B
Chevron Phillips MD6800 HIPS - High Impact Polystyrene  (discontinued **)
Rubber modified high impact polystyrene.Applications:Displays and retail product shelvingDurable household applicationsThin to medium thickness parts that require a combination of high flow and good..
Flexural Modulus 1.95 GPa
283 ksi
ASTM D790
Kostat 5000 TAB Spacer Tapes PET
5000 TAB Spacer Tapes, uniquely formulated and manufactured by KOSTAT, are made of various thermoplastic substrates with ICP (Inherently Conductive Polymer) coating technology. This class of materi..
Flexural Modulus 1.95 GPa
283 ksi
ASTM D790
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Flexural Modulus 1.95 GPa
283 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP KL005 Acetal Copolymer
LNP LUBRICOMP* KL005 is a compound based on Acetal Copolymer resin containing 25% PTFE. Added feature of this material is: Wear Resistant.
Flexural Modulus 1.95 GPa
283 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP KL005 Acetal Copolymer (Asia Pacific)
LNP* LUBRICOMP* KL005 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 1.95 GPa
283 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi..
Flexural Modulus 1.95 GPa
283 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi..
Flexural Modulus 1.95 GPa
283 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP 67002XXH PBT+PC
LNP* THERMOCOMP* 67002XXH is a compound based on PBT+PC containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features inc..
Flexural Modulus 1.95 GPa
283 ksi
ISO 178
Styrolution PS 476L HIPS
Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl..
Flexural Modulus 1.95 GPa
283 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA
NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance.
Flexural Modulus 1.95 GPa
283 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific)
NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance.
Flexural Modulus 1.95 GPa
283 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East)
NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance.
Flexural Modulus 1.95 GPa
283 ksi
ISO 178
Solvay TECHNYL® C 536XT PA6, DRY
Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing..
Flexural Modulus 1.95 GPa
283 ksi
ASTM D790
Teknor Apex Sinpolene TPP2020 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 20% Filler by Weight Uses: Appliance Components; Automotive Applications; Housings Forms: Pellets Process..
Flexural Modulus 1.95 GPa
283 ksi
ASTM-D790
Polyram PlusTek RA845 Nylon 6.6, Impact Modified
Improved impact polyamide 6.6 for good resistance to low temp for injection molding applicationsInformation provided by Polyram Ram On Ind.
Flexural Modulus 1.95 GPa
283 ksi
ASTM D790
Total PS CPDS 818 Easy Flow, Non-Deca Polystyrene
Total Petrochemicals Polystyrene 818 is a high heat resistant, high impact Polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacturing of articles which r..
Flexural Modulus 1.95 GPa
283 ksi
ISO 178
Cossa Polimeri ESTABLEND PA 3000 ABS / Nylon 6 Blend
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri..
Flexural Modulus 1.95 GPa
283 ksi
chs 0.05 in/min; ASTM D790
Diamond Polymers DIAMALOY 527 PC/PBT Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 1.95 GPa
283 ksi
15mm/min; ASTM D790
Denka MALECCA K-600 ABS
A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de..
Flexural Modulus 1.95 - 3.25 GPa

@Temperature 60.0 - 120 °C
283 - 471 ksi

@Temperature 140 - 248 °F
Average value: 2.59 GPa Grade Count:1
Overview of materials for Polypropylene with Glass Fiber + Bead Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max..