Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Omni Plastics OmniTech™ ABS GRC10 NA Glass Reinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Manufacturer Omni Plastics
Trade Name OmniTech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omni Plastics OmniTech™ ABS GRC10 NA Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and Improved Optical Clarity.Applications:flame retardant storage containers, static dissipative trays, internally lubricated gears and rollers, and NSF compliant pool and filler components. Information provided by Omni Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Flexural Modulus 4.00 GPa
580 ksi
ASTM D790
Izod Impact, Notched 0.779 J/cm
1.46 ft-lb/in
ASTM D256