Garlock Viton® 501 Fluoroelastomer Sheet Rubber

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name Viton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock Viton® 501 Fluoroelastomer Sheet Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Style #501 sheet rubber, made with VITON® fluoroelastomer, is a high-performance product resistant to heat, oils, fuels, numerous acids and other chemicals.Information provided by Garlock Rubber TechnologiesViton is a registered trademark of DuPont
Physical Properties Metric English Comments
Specific Gravity 1.85 g/cc
1.85 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 80
70 - 80
85 - 95

@Treatment Temp. 250 °C,
Time 252000 sec
85 - 95

@Treatment Temp. 482 °F,
Time 70.0 hour
Heat Aged
Tensile Strength >= 6.89 MPa
>= 1000 psi
8.96 MPa
1300 psi
Typical
Elongation at Break >= 175 %
>= 175 %
>= 125 %

@Treatment Temp. 250 °C,
Time 252000 sec
>= 125 %

@Treatment Temp. 482 °F,
Time 70.0 hour
Heat Aged; ASTM D573
Compression Set 50 %

@Temperature 175 °C,
Time 79200 sec
50 %

@Temperature 347 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -26.1 °C
-15.0 °F