Old Hickory M-44 Kentucky Ball Clay

Category Ceramic , Clay , Ball Clay
Manufacturer Old Hickory Clay Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Old Hickory M-44 Kentucky Ball Clay.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A highly plastic clay blend containing kaolin and other mixed layer minerals. It is white firing with excellent vitrification properties for use in whiteware ceramic casting, pressing, or plastic forming compositions.Information provided by Old Hickory Clay Company
Physical Properties Metric English Comments
Particle Size 0.50 µm
0.50 µm
44% of particles less than
0.73 µm
0.73 µm
Median particle diameter
1.0 µm
1.0 µm
58% of particles less than
<= 5.0 µm
<= 5.0 µm
83% of particles less than
pH 6.0
6.0
Soluble Sulfates 285 ppm
285 ppm
Specific Surface Area 25.6 m²/g
25.6 m²/g
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00531 GPa
0.770 ksi
Dry Modulus of Rupture for 50% clay/50% flint, cast bars
Thermal Properties Metric English Comments
Shrinkage 5.0 %
5.0 %
Cone 04, Linear Fired Shrinkage
5.8 %
5.8 %
Cone 3, Linear Fired Shrinkage
6.7 %
6.7 %
Cone 11, Linear Fired Shrinkage
6.8 %
6.8 %
Linear Drying Shrinkage
Component Elements Properties Metric English Comments
Al2O3 27.5 %
27.5 %
CaO 0.19 %
0.19 %
Fe2O3 1.62 %
1.62 %
K2O 1.24 %
1.24 %
Loss on Ignition(%) 9.59 %
9.59 %
MgO 0.59 %
0.59 %
Na2O 0.10 %
0.10 %
SiO2 57.68 %
57.68 %
TiO2 1.5 %
1.5 %
Descriptive Properties Value Comments
Absorption (%) 10.1
Cone 04, Fired
3.6
Cone 11, Fired
8.6
Cone 3, Fired
CEC/MBI (meg/100 ml) 10.4
Crude Color Light Grey
Filtration (ml) 19
Pyrometric Cone Equivalent (PCE) 31
Water of Plasticity (%) 33
Wet Sieve Residue (%) 1.04
Wet Sieve Residue, +200 mesh