Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00531 GPa | 0.770 ksi | Dry Modulus of Rupture for 50% clay/50% flint, cast bars |
Old Hickory M-44 Kentucky Ball Clay A highly plastic clay blend containing kaolin and other mixed layer minerals. It is white firing with excellent vitrification properties for use in whiteware ceramic casting, pressing, or plastic fo.. |
|||
Modulus of Rupture | 0.00531 GPa | 0.770 ksi | Dry Modulus of Rupture, 50% clay/50% flint, cast bars |
Old Hickory No. 28 Kentucky Ball Clay This is a kaolin grade with exceptional plasticity, dry and green strength, and low levels of carbon content. it can be utilized in extruded or pressed ceramic formulations and is a clay particularl.. |