Polymer Property : Modulus of Rupture = 0.770 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00531 GPa
0.770 ksi
Dry Modulus of Rupture for 50% clay/50% flint, cast bars
Old Hickory M-44 Kentucky Ball Clay
A highly plastic clay blend containing kaolin and other mixed layer minerals. It is white firing with excellent vitrification properties for use in whiteware ceramic casting, pressing, or plastic fo..
Modulus of Rupture 0.00531 GPa
0.770 ksi
Dry Modulus of Rupture, 50% clay/50% flint, cast bars
Old Hickory No. 28 Kentucky Ball Clay
This is a kaolin grade with exceptional plasticity, dry and green strength, and low levels of carbon content. it can be utilized in extruded or pressed ceramic formulations and is a clay particularl..