Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 49.6 MPa | 7190 psi | ASTM D638 |
Plaskolite Optix® CA-927 HF Clear Impact Modified Acrylic Resin Impact modified acrylic resin, injection molding gradeApplications: A high flow, impact-modified acrylic resin for injection molding. This resin offers impact strengths up to seven times those of g.. |
|||
Tensile Strength, Ultimate | 49.6 MPa | 7190 psi | ASTM D638 |
Plaskolite West Optix® CA-927 HF Clear Impact Modified Acrylic Resin Impact modified acrylic resin, injection molding gradeApplications: A high flow, impact-modified acrylic resin for injection molding. This resin offers impact strengths up to seven times those of g.. |
|||
Tensile Strength, Ultimate | 49.6 MPa | 7200 psi | ASTM D638 |
Nylene® Naxel™ B720 Polycarbonate/PBT Alloy Description: Naxel™ B720 is a Polycarbonate/PBT alloy. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Tensile Strength, Ultimate | 49.6 MPa | 7190 psi | ASTM D638 |
Plaskolite West Optix® CA-927 G HF Clear Impact Modified Acrylic Resin Impact modified acrylic resin, injection molding gradeApplications: A high flow, impact-modified acrylic resin designed for medical or food uses. This resin offers impact strengths up to seven time.. |
|||
Tensile Strength, Ultimate | 49.6 - 110 MPa | 7200 - 16000 psi | Average value: 71.1 MPa Grade Count:12 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Tensile Strength, Ultimate | 49.6 MPa | 7200 psi | ASTM D638 |
Global GAB-105 5% Glass Reinforced ABS Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Ultimate | 49.6 MPa | 7200 psi | |
BCC Products BC 6060 Epoxy Surface Coat/Casting BC 6060 is a blue epoxy, abrasion resistant surfacing resin. Commonly referred to as “die surface” material, this system may be applied by brush or if preferred, cast in thin sections to a maximum.. |
|||
Tensile Strength, Ultimate | 49.6 MPa | 7200 psi | |
BCC Products BC 7053 Epoxy Casting BC 7053 is an iron filled epoxy casting system. This system is a high iron content material that provides unsurpassed wear resistance. BC7053 was designed for use in constructing core boxes, holding.. |
|||
Tensile Strength, Ultimate | 49.6 - 400 MPa | 7200 - 58000 psi | Average value: 132 MPa Grade Count:34 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |