Nylene® 451 Nylon 6, 50% RH

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 451 Nylon 6, 50% RH.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection molding grade. Nylene 451 is recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistance insure long product life to gears, bearings, cams, fasteners, and other load bearing parts. Nylene 451 chemically resists oil and grease.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Yield Strength 28.0 MPa
4060 psi
ASTM D790
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 238 - 249 °C
460 - 480 °F
At Nozzle
Nozzle Temperature 238 - 249 °C
460 - 480 °F