Nye Lubricants 785G (NG) Synthetic Oil

Category Fluid , Lubricant , Silica Gellant , Silicone Base
Manufacturer Nye Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 785G (NG) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Evaporation Loss 1.3 %
1.3 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Oil Separation 1.3 %
1.3 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Recommended
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Recommended
Pour Point -50.0 °C
-58.0 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type Sil.(Dimeth)
Gellant Type Silica (WR)