Polymer Property : Melting Point = 181 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 181 - 290 °C
358 - 554 °F
Average value: 217 °C Grade Count:3
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Melting Point 181 °C
358 °F
Noltex Soarnol® MS3203 Ethylene Vinyl Alcohol Copolymer
Modified DC3203; New improved thermoformable EVOH. Ethylene content 32 mol%.Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon ..
Melting Point 181 °C
358 °F
DSC
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan..
Melting Point 181 °C
358 °F
DSC
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL..
Melting Point 181 - 187 °C
358 - 369 °F
Indium Corp. Indalloy 226 Tin Solder Alloy
Zinc causes high dross U.S. Patent #5,242,658; covers 72.8-89.4Sn 6.7-19.2Zn 2.7-16.4In; temp. range Liq.. 176-193, Sol. 166-191.4Information Provided by Indium Corporation
Melting Point 181 °C
358 °F
DSC
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket..
Melting Point <= 181 °C
<= 358 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 726.07 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. LD 716.07 is an excelle..
Melting Point <= 181 °C
<= 358 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ UL 15019CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 15019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: Hot..
Melting Point 181 °C
358 °F
ASTM D3418
ALM PA 250 Nylon 12 SLS Prototyping Polymer
Highly Recyclable Nylon 12 Laser Sintering Material.Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or..
Melting Point 181 °C
358 °F
ASTM D3418
ALM PA 605-A Filled Nylon 12 Prototyping Polymer
50% Aluminum filled nylon 12 that can produce accurate parts with excellent part strength and surface detail.Drop in replacement for other commercially available 50% aluminum filled materials with a..
Melting Point 181 °C
358 °F
ASTM D3418
Ashley Polymers Ashlene® PPO Resin P259
A high flow grade for applications requiring high impact strength and a high heat deflection temperature.Data provided by the manufacturer
Melting Point 181 °C
358 °F
ASTM D3418
ALM PA 606-FR Filled Nylon 12 Prototyping Polymer
Only commercially available fire retardant nylon 12 material, which meets FAR 25.853 60 second burn specification.The parts produced from PA 606-FR have a much smoother surface finish and sharper fe..
Melting Point 181 °C
358 °F
ASTM D3418
ALM PA 650 Nylon 12 SLS Prototyping Polymer
Combines strength, durability (high impact) and chemical resistance and produces strong, durable, end use prototype parts. SL parts are less porous, more precise and have less noticeable build lines..
Melting Point 181 °C
358 °F
DSC
EVALCA EVAL® EF-XL Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
Biaxially oriented type film; property values for 15 µm film.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produ..
Melting Point 181 °C
358 °F
DSC
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro..
Melting Point 181 °C
358 °F
ASTM D3418
Ashley Polymers Ashlene® P258 PPO
A high flow grade for applications requiring good impact strength and a high heat deflection temperature.Data provided by the manufacturer