| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.82 g/cc | 1.82 g/cc | ASTM D792 |
| Melt Flow | 19.35 g/10 min @Load 2.16 kg, Temperature 230 °C |
19.35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 80 | 80 | ASTM D2240 |
| Tensile Strength at Break | 2.95 MPa | 428 psi | ASTM D412 |
| Elongation at Break | 132 % | 132 % | ASTM D412 |
| 2% Secant Modulus | 0.05904 GPa | 8.563 ksi | ASTM D790 |
| Tear Strength | 42.72 kN/m | 243.7 pli | ASTM D624 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 191 - 218 °C | 375 - 425 °F | |