Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 42.72 kN/m | 243.7 pli | ASTM D624 |
Noble Polymers Ecobarrierâ„¢ 0918 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |