Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers Softflex® 8800

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Network Polymers
Trade Name Softflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers Softflex® 8800.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Melt Flow 3.0 g/10 min

@Load 1.00 kg,
Temperature 235 °C
3.0 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 80 - 90
80 - 90
10 second dwell; ASTM D2240
83 - 93
83 - 93
Instantaneous; ASTM D2240
Tensile Strength, Yield 15.2 MPa
2200 psi
chs 20 in/min; ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
Flexural Modulus 0.352 GPa
51.0 ksi
Compression Set 47.7 %
47.7 %
Method B, 22 hours at 25% deflection and 23°C; ASTM D395
97.8 %

@Temperature 70.0 °C
97.8 %

@Temperature 158 °F
22 hours at 25% deflection; ASTM D395, Method B,
100 %

@Temperature 100 °C
100 %

@Temperature 212 °F
22 hours at 25% deflection; ASTM D395, Method B,
Users viewing this material also viewed the following: