Polymer Property : Flexural Modulus = 51.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.352 GPa
51.0 ksi
Network Polymers Softflex® 8800
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Flexural Modulus 0.352 GPa
51.0 ksi
ASTM D 790
Shakespeare Isocorâ„¢ TT52SI Nylon 6 Terpolymer
Isocorâ„¢ TT52SI multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Isocorâ„¢ TT52SI is easily processed and has a wide range of application..