Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers NPP 30-1200 TF20

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP 30-1200 TF20.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: 20% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 8.0 - 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 - 12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Yield 31.0 MPa
4500 psi
2 in per min, tangent; ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
6.00 ft-lb/in
ASTM D256
Gardner Impact 0.569 J
0.420 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved