NatureWorks® Ingeo™ 6350D Fiber Grade PLA

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polylactic Acid (PLA) Biopolymer
Manufacturer NatureWorks LLC
Trade Name Ingeo™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NatureWorks® Ingeo™ 6350D Fiber Grade PLA.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
NatureWorks PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into spunbond nonwovens using conventional bi-component PET spunbond equipment, where filament velocities > 4000 m/min can be achieved. NatureWorks PLA 6350D can be used as a low melt binder polymer in a sheath-core confiation. Potential applications for PLA polymer 6350D include bicomponent spunbond non-wovens
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Melt Density 1.08 g/cc

@Temperature 230 °C
0.0390 lb/in³

@Temperature 446 °F
ASTM D1238
Viscosity Measurement 2.5
2.5
Relative Viscosity; CD Internal Viscotek Method
Melt Flow 65 g/10 min

@Load 2.16 kg,
Temperature 210 °C
65 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 145 - 160 °C
293 - 320 °F
ASTM D3418
Glass Transition Temp, Tg 55.0 - 60.0 °C
131 - 140 °F
ASTM D3417
Processing Properties Metric English Comments
Dew Point -35.0 °C
-31.0 °F
Drying Air Flow Rate >= 14.2 l/min
>= 0.500 ft³/min (CFM)