Material Notes:
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when PP is produced, processed and PP-made articles are exploited, effective nucleation, improved optical properties, improved antistatic properties to produce articles, and improved rheology of melt.Information provided by manufacturer
Physical Properties Metric English Comments
Melt Flow 40 - 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
40 - 45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
Mechanical Properties Metric English Comments
Flexural Modulus >= 0.950 GPa
>= 138 ksi
ASTM D790
Izod Impact, Notched >= 0.450 J/cm
>= 0.843 ft-lb/in
ASTM D256