NIZHNEKAMSKNEFTEKHIM PP 1315M (YX37F) Propylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PP 1315M (YX37F) Propylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when PP is produced, improving properties contributing to slipping and preventing from film layers sticking, improved rheology of melt.Information provided by manufacturer
Physical Properties Metric English Comments
Melt Flow 7.5 - 10.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.5 - 10.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 31.0 MPa
>= 4500 psi
ASTM D256
Elongation at Yield >= 10 %
>= 10 %
ASTM D638
Flexural Modulus >= 1.20 GPa
>= 174 ksi
ASTM D790
Descriptive Properties Value Comments
Gel Content (pcs./m²) 0
>= 2.5mm
0
(1.5-2.5)mm
250
>=0.2mm
3
(0.7-1.5)mm