Material Notes:
Grade 825EF is a high impact polystyrene designed for extrusion and hot molding application. It is suited for hot molded deep drawn industrial packages and multilayer shaped sheet production via extrusion. Resistant to cyclopentane effect.Information provided by manufacturer
Physical Properties Metric English Comments
Melt Flow 3.0 - 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 - 5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 20.0 MPa
>= 2900 psi
ASTM D638
Elongation at Break >= 45 %
>= 45 %
ASTM D638
Flexural Strength >= 38.0 MPa
>= 5510 psi
ASTM D790
Izod Impact, Notched >= 1.01 J/cm
>= 1.89 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point >= 88.0 °C
>= 190 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 48 %
48 %
60°; ASTM D523
Chemical Properties Metric English Comments
Styrene Content <= 0.050 %
<= 0.050 %
p. 4.10 of the TU