Material Notes:
Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: InteriorInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Ash 30 %
30 %
ASTM D5630
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Yield 25.0 MPa
3630 psi
50 mm/min; ASTM D638
Flexural Modulus 2.60 GPa
377 ksi
Tangent; 1.3 mm/min; ASTM D790
Izod Impact, Notched 0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648