Polymer Property : Tear Strength = 215 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 37.7 kN/m
215 pli
post cured- 2 hours at 177°C; Die B
Multibase SILASTIC® C7-4550 VAROX Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength 37.7 kN/m
215 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N550 (FEF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 37.7 kN/m
215 pli
Fill/Transverse direction
Saint-Gobain Chemlam® 10 Value Industrial Laminate
Description: The Chemlam® series is the Chemfab® value line of industrial laminates. Chemlam® composites features uniform thickness, multi-layer cast PTFE films laminated to fiber glass rei..
Tear Strength 37.7 kN/m
215 pli
Fill/Transverse direction
Saint-Gobain Chemlam® Silver 10 Wear Resistant Industrial Laminate
Description: The Chemlam® Silver series is the wear resistant line of Chemfab® industrial laminates. Chemlam® Silver composites feature uniform thickness, multi-layer cast PTFE films lamina..
Tear Strength 37.7 kN/m
215 pli
ASTM D624
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 65-HR-1 TPE
Product Description: StarTUFF TF 65-HR-1 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M..
Tear Strength 37.7 kN/m
215 pli
JIS K6301-B
Stellarchem MP-950NC TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Tear Strength 37.7 kN/m
215 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N550 (FEF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 37.7 kN/m
215 pli
ASTM D1004
Bayshore Vinyl Compounds BVC 7200-65 Vinyl Compound
BVC 7200-65 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a s..
Tear Strength 37.7 kN/m
215 pli
Axiall 8741 Moldings & Extrusions Flexible PVC
A low gravity general purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axi..