Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ FG 5690Q Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer 3M Dyneon™
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ FG 5690Q Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Dyneon™ Fluoroelastomer FG 5690Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, Dyneon FG 5690Q should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stabilityComposition: Di-polymer of vinylidene fluoride and hexafluoropropyleneHigh mooney version of FG 5630QIn compliance with US FDA 21 CFR 177.2600When compared to diamine cured compounds this product gives excellent mold release, better moInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Mooney Viscosity 97

@Temperature 121 °C
97

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 16.3 MPa
2360 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 200 %
200 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 0.00710 GPa
1.03 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 10 %
10 %
Aged 70 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Transformation Temperature -18.0 °C
-0.400 °F
TR10; ASTM D1329
Component Elements Properties Metric English Comments
Fluorine, F 65.9 %
65.9 %
Descriptive Properties Value Comments
Color Opaque Off-White
MH, Maximum Torque 24.2 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque 3.3 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
Mooney Scorch, MS 0
Point rise at 25 min @ 121°C
Mooney Scorch, MS Minimum 68
@ 121°C
Solubility Ketones and Esters
t`50, Time to 50% cure 3.2 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure 4.3 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ts2 - Time to 2 in-lb rise from min 2.2 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C