Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.55 MPa | 225 psi | 200%, post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4535 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.55 MPa | 225 psi | 200%, post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4550 VAROX Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |