Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 10 g/10 min
10 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 46
46
10 sec; ASTM D-2240
Tensile Strength, Ultimate 15.2 MPa
2200 psi
ASTM D412
Elongation at Break 125 %
125 %
ASTM D412
Flexural Modulus 0.531 GPa
77.0 ksi
method 1, Proc.B; ASTM D-790
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D3029
Tear Strength 100.7 kN/m
574.6 pli
ASTM D624