Polymer Property : Gardner Impact = 22.6 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products FT2600-677UV Thermoplastic Polyolefin, UV Stabilized, 0848 Black
Applications: Exterior trimStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products FT4650-583UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black
Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products HP521-00UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural
Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral
Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products HP521-372 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter
Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products P252-01 Polypropylene Copolymer, Black
Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products P256-00 Polypropylene Copolymer, Natural
Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J

@Temperature -30.0 °C
16.7 ft-lb

@Temperature -22.0 °F
Gardner
Network Polymers NPP 25-0803
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Gardner Impact 22.6 J

@Temperature -18.0 °C
16.7 ft-lb

@Temperature -0.400 °F
Network Polymers NPP 25-1002
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D3029
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified
General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples...
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D3029
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D3029
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Gardner Impact >= 22.6 J
>= 16.7 ft-lb
ASTM D3029
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D3029
Polymer Resources PPX-FR7 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 260F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products HP521-288UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167A Ebony
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D5420
RheTech Products HP522-286 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZUCA Medium Graphite
Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 22.6 J
16.7 ft-lb
ASTM D3029
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Gardner Impact 22.6 - 22.6 J
16.7 - 16.7 ft-lb
Average value: 22.6 J Grade Count:5
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Gardner Impact 22.6 J

@Thickness 3.17 mm
16.7 ft-lb

@Thickness 0.125 in
ASTM D3029
Ineos Styrenics Polystyrene 476M (NAFTA)
High-impact grade of polystyrene with good ESCR designed to provide uniform melt flow for excellent processability.Information provided by BASF.Ineos Styrenics purchased this product line from BASF ..
Gardner Impact 22.6 J

@Temperature -30.0 °C
16.7 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer
DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de..
Gardner Impact 22.6 J

@Temperature 23.0 °C
16.7 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 67 mil
Axiall MP-6510 Rigid PVC, Molding
Georgia Gulf MP-6510 is a maximum properties electrical grade PVC injection molding compound processing excellent strength and toughness. In addition, it has good processing stability and surface a..
Gardner Impact >= 22.6 J
>= 16.7 ft-lb
ASTM D3029
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength  (Unverified Data**)
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Gardner Impact >= 22.6 J
>= 16.7 ft-lb
ASTM D3029
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Walled Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Gardner Impact >= 22.6 J
>= 16.7 ft-lb
ASTM D3029
Polymer Resources PPX-FR7 Modified PPO, V-0 Flame Retardant, Medium Heat, 250 HDT  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.