Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.531 GPa | 77.0 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE D 4510 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.531 GPa | 77.0 ksi | ASTM D790 |
Quadrant EPP TIVAR® HPV UHMW-PE (ASTM Product Data Sheet) |