Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE D 4210 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE D 4210 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.87 g/cc
0.0676 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 8.0 - 15 g/10 min
8.0 - 15 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 38
38
10 sec; ASTM D-2240
Tensile Strength, Ultimate >= 4.50 MPa
>= 653 psi
ASTM D412
Elongation at Break >= 190 %
>= 190 %
ASTM D412
Flexural Modulus 0.241 GPa
35.0 ksi
method 1, Proc.B; ASTM D-790
Tear Strength >= 27.2 kN/m
>= 155 pli
ASTM D624
Users viewing this material also viewed the following: