Polymer Property : Specific Gravity = 1.92 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.92 g/cc
1.92 g/cc
Slurry
Omya OMYACARB® UF - FL Calcium Carbonate
A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water..
Specific Gravity 1.92 g/cc
1.92 g/cc
Omya OMYAFLOW® UF - SY Calcium Carbonate
A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Decorative paints.Information supplied by Omya North America.
Specific Gravity 1.92 g/cc
1.92 g/cc
ASTM D297
Greene Tweed CHEMRAZ® 510 Perfluoroelastomer
Greene Tweed’s Chemraz® 510, a perfluoroelastomer, offers an extremely broad range of chemical resistance with a Shore A hardness value of 90. with a temperature range form -22°F to 446Â..
Specific Gravity 1.92 g/cc
1.92 g/cc
ASTM D297
Greene Tweed CHEMRAZ® 526 Perfluoroelastomer
Greene Tweed’s Chemraz® 526, a perfluoroelastomer, offers superior chemical compatibility coupled with explosive decompression resistance, making it the ideal compound for fluid handling equ..
Specific Gravity 1.92 g/cc
1.92 g/cc
ASTM 792
Multibase Multi-Flex® 8832 C Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Specific Gravity 1.92 g/cc
1.92 g/cc
ASTM 792
Multibase Multi-Flex® A 8832 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Noise Damping Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation provided by Mult..
Specific Gravity 1.92 g/cc
1.92 g/cc
ASTM D297, 15
Seals Eastern 5723 Fluorocarbon-Elastomer
Formulated Viton®. General service.Information provided by Seals Eastern, Inc.
Specific Gravity 1.92 g/cc
1.92 g/cc
ASTM D297, 15
Seals Eastern 7130 Fluorocarbon-Elastomer
FKM specially for oil & gas service.Information provided by Seals Eastern, Inc.
Specific Gravity 1.92 g/cc
1.92 g/cc
at 25°C
Daikin DAI-EL G-501NK Fluoroelastomer Terpolymer, Diamine Curable Grade, 68% Fluorine Content
Features: Good mechanical characteristics.Information provided by Daikin Industries.
Specific Gravity 1.92 g/cc
1.92 g/cc
at 25°C
Daikin DAI-EL G-603 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 71% Fluorine Content
Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Information provided by Daikin Industries.
Specific Gravity 1.92 g/cc
1.92 g/cc
at 25°C
Daikin DAI-EL G-621 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 71% Fluorine Content
Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: General purpose with excellent sol..