Material Notes:
Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionBlow MoldingUses:TubingPipingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
Flexural Modulus 0.689 GPa
100 ksi
ASTM D790
Izod Impact, Notched 2.94 J/cm
5.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
0.125 in